Shampoo

Fluffy Foam Shampoo

Phase Ingredient INCI Purpose %
A - Water - Balance
- Polyquaternium-10 Conditioning, Thickener 0.50
B NISSAN ANON™ BDF-R Cocamidopropyl Betaine, Water Improve detergency, foam quality 20.00
PERSOFT™ EF Sodium Laureth Sulfate, Water Improve detergency, foam quality 10.00
DIAPON™ K-SF Sodium Methyl Cocoyl Taurate, Water Improve detergency, foam quality 10.00
SOFTILT™ AS-L Sodium Lauroyl Methylaminopropionate, Water Improve detergency, Thickener 10.00
NONION™ DL-40HN(W) PEG-75 Dilaurate, Water Thickener, Improve foam volume 2.00
MACBIOBRIDE™ MG-T PEG-120 Methylglucose Triisostearate, Water Thickener 0.60
UNISAFE™ PGML Propylene Glycol Laurate Thickener 0.50
Preservative - Preservative q.s.
C - Citric Acid pH adjuster q.s.
D NONION™OT-221 Polysorbate 80 Solubilizer 0.80
- Fragrance - q.s.

Typical Physical Properties : pH (Undiluted Solution) 6.0, Viscosity (Undiluted Solution, 25 ℃) 3,000~5,000 mPa・s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.
This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

Rich Foam Non-silicon Shampoo

Phase Ingredient INCI Purpose %
A - Water - Balance
- Polyquaternium-10 Conditioning, Thickener 0.50
B NISSAN ANON™ BDF-R Cocamidopropyl Betaine, Water Improve detergency, foam quality 16.70
PERSOFT™ EF Sodium Laureth Sulfate, Water Improve detergency, foam quality 16.40
LUMINOVEIL™ HS-L Sodium Lauroyl Hydroxyethyl Beta-alaninate, Water Improve detergency, foam elasticity 3.00
RG・CO・P™ Glycerin Moisturizer 2.00
STAFOAM™DL Lauramide DEA Thickener, Improve foam volume 1.50
LIPIDURE®-C Polyquaternium-64, Water, Phenoxyethanol Conditioning 0.10
- Glycosyl Trehalose Moisturizer 0.10
Preservative - Preservative q.s.
C - Citric Acid pH adjuster q.s.
D NONION™OT-221 Polysorbate 80 Solubilizer 0.80
- Fragrance - q.s.

Typical Physical Properties : pH (Undiluted Solution) 6.0, Viscosity (Undiluted Solution, 25 ℃) 870 mPa・s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.
This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

High-blending Oil Shampoo

Phase Ingredient INCI Purpose %
A - Water - Balance
- Polyquaternium-10 Conditioning, Thickener 0.25
B LUMINOVEIL™ HS-L Sodium Lauroyl Hydroxyethyl Beta-alaninate, Water Improve detergency,foam quality, foam elasticity 50.00
DIAPON™ HF-SF Sodium Caproyl Methyltaurate, Water Improve foam volume 15.00
NISSAN ANON™ BDF-SF Cocamidopropyl Betaine, Water Improve detergency, foam quality 11.00
Preservative - Preservative q.s.
C UNIOX™ ST-40E Sorbeth-40 Tetraoleate Solubilizer 6.00
- Olea Europaea (Olive) Fruit Oil Conditioning 2.00
- Argania Spinosa Kernel Oil Conditioning 1.00
D - Citric Acid pH adjuster q.s.
E NONION™ OT-221 Polysorbate 80 Solubilizer 0.80
- Fragrance - q.s.

Typical Physical Properties : pH (Undiluted Solution) 6.1, Viscosity (Undiluted Solution, 25 ℃) 330 mPa・s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Separately, measure the phase-C ingredients and stir at 80±5 ℃ until evenly mixed.
  4. Add (3) solution to (2) solution and stir until evenly mixed.
  5. Add the phase-D ingredient and stir at 80±5 ℃ until evenly mixed.
  6. After cool down to 25±5 ℃, add the phase-E ingredients before mixed at 25±5 ℃, and stir until evenly mixed.
This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

Moist Shampoo

Phase Ingredient INCI Purpose %
A - Water - Balance
- Polyquaternium-10 Conditioning, Thickener 1.20
B DIAPON™ K-SG Sodium Taurine Cocoyl Methyltaurate, Water Improve detergency,
foam quality, Moisturizer
18.60
NISSAN ANON™ BDF-SF Cocamidopropyl Betaine, Water Improve detergency,
foam quality
15.00
SOFTILT™ AS-L Sodium Lauroyl Methylaminopropionate, Water Improve detergency, Thickener 11.00
- Dipropylene Glycol Moisturizer 4.00
- Butylene Glycol Moisturizer 2.00
- Caprylyl/Capryl Glucoside Improve foam volume 2.00
- Disodium Cocoyl Glutamate Improve foam volume 1.50
STAFOAM™ DL Lauramide DEA Thickener, Improve foam volume 0.90
Preservative - Preservative q.s.
C - Citric Acid pH adjuster q.s.
D NONION™OT-221 Polysorbate 80 Solubilizer 0.80
- Fragrance - q.s.

Typical Physical Properties : pH (Undiluted Solution) 5.9, Viscosity (Undiluted Solution, 25 ℃) 1,450 mPa・s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.
This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

Smooth and Volume-rich Shampoo

Phase Ingredient INCI Purpose %
A - Water - Balance
- Polyquaternium-10, Polyquaternium-7 Conditioning, Thickener 0.90
B DIAPON™K-SF Sodium Methyl Cocoyl Taurate, Water Improve detergency, foam quality 30.00
NISSAN ANON™ BL-SF Lauryl Betaine, Water Improve detergency, foam quality 15.00
SOFTILT™ AX-L Sodium Taurine Lauroyl Methyl Beta-alaninate, Water Improve detergency, Thickener 4.80
NISSAN ANON™ LA Disodium Lauriminodiacetate, Water Improve detergency, foam quality 4.20
NONION™ DL-40HN(W) PEG-75 Dilaurate, Water Thickener, Improve foam volume 2.00
- Dipropylene Glycol Moisturizer 2.00
STAFOAM™ MF Cocamide MEA Thickener, Improve foam volume 0.80
- Disodium Cocoyl Glutamate Improve foam volume 0.50
Preservative - Preservative q.s.
C - Citric Acid pH adjuster q.s.
D NONION™OT-221 Polysorbate 80 Solubilizer 0.80
- Fragrance - q.s.

Typical Physical Properties : pH (Undiluted Solution) 5.7, Viscosity (Undiluted Solution, 25 ℃) 370 mPa・s

Preparation Method

  1. Measure the phase-A ingredients and stir at room temperature until evenly mixed.
  2. Heat the phase-A ingredients to 80±5 ℃ and add the phase-B ingredients.
  3. Add the phase-C ingredient and stir at 80±5 ℃ until evenly mixed.
  4. After cool down to 25±5 ℃, add the phase-D ingredients before mixed at 25±5 ℃, and stir until evenly mixed.
This formula is result by our best efforts. But, this formula does not guarantee performance, safety, stability, or commercial property rights for your products.

PAGE TOP